Hi Expert,

Does anyone know the supplier/manufacturer (or its material) who produce/develope the coating material to the boiler tube for the purpose of anti-slagging from poor quality of lignite coal fuel? Or even to delay the slag froming rate would be appreciated.

We used to try the lignite coal additive to alliviate the slag forming problem but it doesn't work.

Regards,