HI, EVERYBODY,
I RUN INTO A PROBLEM HOPING SOMEONE CAN HELP ME DETERMINE WHAT MIGHT BE THE CAUSE OF THAT.
I JUST RECEIVED PARTS BACK FROM PASSIVATION WHICH HAVE LOOSE PITCH BLACK POWDER ALL OVER THE PARTS. THE POWDER CAN BE SMEARED OFF EASILY.
MATERIAL IS 440C, ROUGH MACHINED PRIOR TO HEAT TREATED TO Rc54~56, SEVERAL GRINDING OPERATIONS AFTER THAT. THEN GET MAGNETIC INSPECTED AND PASSIVATED.
THANK YOU ALL IN ADVANCE.
I RUN INTO A PROBLEM HOPING SOMEONE CAN HELP ME DETERMINE WHAT MIGHT BE THE CAUSE OF THAT.
I JUST RECEIVED PARTS BACK FROM PASSIVATION WHICH HAVE LOOSE PITCH BLACK POWDER ALL OVER THE PARTS. THE POWDER CAN BE SMEARED OFF EASILY.
MATERIAL IS 440C, ROUGH MACHINED PRIOR TO HEAT TREATED TO Rc54~56, SEVERAL GRINDING OPERATIONS AFTER THAT. THEN GET MAGNETIC INSPECTED AND PASSIVATED.
THANK YOU ALL IN ADVANCE.