I need a recommendation for a adhesive that will bind tyvek and mylar into a two ply material. UV will not be an issue because the mylar will be aluminized. But heat will be, as the final product will be used as a desert shade structure material. The end result needs to be flexable so the material can be rolled for transportation. Low/no shrinkage is also obvously important. Each piece of final material will be at most 3m x 3m. The prototypes will be built in the next few days and will about 400 sq/ft, so imeadiate availabity of small quanities is nessasary. Spray application is perferable, but anything will be concidered.

Thanks in advance for the help.

~ Shawn
 
You could sew them together?

Not sure about temperature resistance, but there is a sprayable rubber cement called SprayTack?

TTFN

 

Google - reflektra - for a similar ready made product?
 