Can you advice about the best type of adsorbant commonly used to adsorb mercaptans from light hydrocarbon products

thanks advanced.
 
Replies continue below

Recommended for you

Typically 5A may be used. Visit UOP website for more details.

Samiran
 
etoile
A very helpful person at UOP is Jack Corvini. You can e-mail him at gcorvini@uop.com

Hope this helps.
 