Sep 25, 2001 #1 tedg Materials Joined Dec 23, 2000 Messages 34 Location US Can anyone tell me the composition and properties of a beryllium copper alloy identified as NSB4? Is this a foreign standard? Where can we buy the alloy? Is there an equivalent North American alloy? Any information would be much appreciated.
Can anyone tell me the composition and properties of a beryllium copper alloy identified as NSB4? Is this a foreign standard? Where can we buy the alloy? Is there an equivalent North American alloy? Any information would be much appreciated.
Oct 10, 2001 #2 Brush Electrical Joined Apr 7, 2003 Messages 1 Location US I would suggest contacting Brush-Wellman, a manufacturer of Be containing alloys. They have a website, but I dont know the name of it. Im sure they will have the information you need. Upvote 0 Downvote
I would suggest contacting Brush-Wellman, a manufacturer of Be containing alloys. They have a website, but I dont know the name of it. Im sure they will have the information you need.
Oct 11, 2001 #3 GRPatel Electrical Joined Aug 10, 2001 Messages 40 Location IN Other supplier of the BeCu shaped materials id NGK of Japan.You may approach them. They have offices in US also. Upvote 0 Downvote
Other supplier of the BeCu shaped materials id NGK of Japan.You may approach them. They have offices in US also.