Apr 7, 2010 #1 answerseek Mechanical Joined Apr 7, 2010 Messages 3 Location US hello, where would I find bend radius for c17200 td04 .040" thick? thank you
Apr 7, 2010 #2 berkshire New member Joined Jun 8, 2005 Messages 4,429 Location US answerseek, Why don't you google it? I got 9 hits in 10 seconds. here is one of them. http://www.brushwellman.com/WorkArea/downloadasset.aspx?id=346 B.E. Upvote 0 Downvote
answerseek, Why don't you google it? I got 9 hits in 10 seconds. here is one of them. http://www.brushwellman.com/WorkArea/downloadasset.aspx?id=346 B.E.
Apr 7, 2010 #3 CorBlimeyLimey Mechanical Joined Nov 5, 2003 Messages 15,292 Location CA In the bent part? Assuming you mean the minimum recommended bend radius http://www.brushwellman.com/WorkArea/downloadasset.aspx?id=346 http://lmgtfy.com/?q=minimum+recommended+bend+radius+for+beryllium+copper Upvote 0 Downvote
In the bent part? Assuming you mean the minimum recommended bend radius http://www.brushwellman.com/WorkArea/downloadasset.aspx?id=346 http://lmgtfy.com/?q=minimum+recommended+bend+radius+for+beryllium+copper
Apr 7, 2010 #4 berkshire New member Joined Jun 8, 2005 Messages 4,429 Location US CBL As one limey to another I see we think alike. B.E. Upvote 0 Downvote
Apr 7, 2010 #5 CorBlimeyLimey Mechanical Joined Nov 5, 2003 Messages 15,292 Location CA Hmmm ... a comforting and yet scary thought. Upvote 0 Downvote