Hi guys,

I need an info on Belleville washers. I want to know what is the max number of times a single belleville washer can be used/reused. I want to know this because the mechanics where I work were once told to only use the same washer twice. We have a LOT of washers here and I wonder if they could use them more than 2 times.

Thanks a lot for your time,

Simon
 
Replies continue below

Recommended for you

sounds like a question for the manufacturer about specific part numbers.

then there may be a problem of keeping track of how many time they have been re-used
 
I just did a simple Google search and turned up many instances where the manufactures of Belleville Washers go out of their way to promote the idea that they have done extensive fatigue testing and they assure the buyer that their products are resistant to fatigue failure.

Based on this impression, it would appear that this is an issue which the manufactures are talking about without really being prompted to do and as such it suggests a couple of things. 1) it feels as if there has been problems in the past, which could very well explain why your mechanics warned you about this, but 2) it would also appear that the manufactures may have responded to this by producing better products and backing them up with test data. I would say that Tmoose might have the right idea, check with the manufacture of the washers that you're using and see what they have to say about the fatigue life of their particular products.

John R. Baker, P.E.
Product 'Evangelist'
Product Design Solutions
Siemens PLM Software Inc.
Industry Sector
Cypress, CA
UG/NX Museum:
To an Engineer, the glass is twice as big as it needs to be.
 
it'd depend on whether the washer has been deformed ... no?
 
Thanks a lot guys for your answers, I will contact my supplier to have more info!

Thank again
 
There are a tremendous amount of computational engines for stress analysis on the web. Your issue is one of cyclic loading and lifetime. You can definitely re-use a Belleville Washer stack more than twice, depending on your application. In my experience, rare to use them only twice, probably a mis-spec of the application. They are way more reliable than that!

Do the research and ensure the Belleville Washer application suits the components needed.

Kenneth J Hueston, PEng
Principal
Sturni-Hueston Engineering Inc
Edmonton, Alberta Canada
 
I would definately follow the advice posted above about contacting you spring manufacturer for information on the specific characteristics of your spring as there are numerous designs for different applications.

If you want to educate yourself on the application and design of disk spring components here is a link to the Schnoor handbook.

Key Bellevilles has a CD for the design and application of disk springs

 
trudels,

Roark's Equations has a section explaining Belleville washers. You can work out the stress for yourself, and analyse for fatigue. They are springs. They are under a lot of stress.

Critter.gif
JHG
 
I used to work with machine tools and they are often used to securely hold tools in place. These tools could be subjected to 'tool changes' many hundreds of times per shift. This would constantly be putting the washers under stress/fatigue. In seven years I didn't have to replace a single one.

That said I have seen failures with them in my current job, but they are subjected to far greater forces (400 Tonne presses) and in a harsh environment (concrete products).
 
Agree with Grindy. We own many CNC machines and have rebuilt many draw bar systems that retain a machine tool holder in the spindle. It is very common to get approx 100,000 tool changes without issue. They are usually compounded in series and parallel to achieve a target amount of travel and force. They are usually compressed to max every time, then released BUT they are usually at about 20-40% of compression when released so they retain a draw force on the tool when running in the spindle.

IMO, you can get a lot of cycles from them. IMO, the nasty vibrations and harmonics from machining largely contributes to the failure of the washers, not just the fatigue limits.
 
I know of a product where belleville washers are used as spring packs for actuators where the actuator can and often does drive into the spring pack when subjected to high operating torque. The flexure of the spring pack allows the mechanism to flex so that a torque switch can be made (or broken) when the flexure exceeds a preset value.

These washers flex to some extent every time the actuator operates if it is operating at or near its rated torque and only flex to the maximum extent so as to trip the torque switch if the design torque value is exceeded.

These belleville washers certainly are "reused" time and time again without ever being disassembled.

rmw
 
My 1983 Honda VF750F uses a belleville washer to clamp the clutch pack. Still working fine after 28 years.

The Help for this program was created in Windows Help format, which depends on a feature that isn't included in this version of Windows.
 
A lot depends on your type of application and requirement for reliability. In race cars, teams typically use new parts everytime they rebuild the car between races. Might be excesssive and waste some good parts, but they can't afford any chances. Nuts, bolts and washers are the most common parts that are not reused.


"Wildfires are dangerous, hard to control, and economically catastrophic."

Ben Loosli
 
Tend to agree with looslib...

The mfg will probably say change them every time - since they are in the business of "selling" them.

For non-critical apps - I am sure they can be re-used. But if you are building space shuttles or holding jet engines on airplanes or building race cars - I think I would use new ones every time.
 
Sometimes NEW = Never Ever Worked (before), especially in this age of components from suppliers from far away. Not that it was all good in the good old days, or sometimes they make 'em much better than they used to, but..............

Some moderately strict MIL spex allow reusing nylon locking nuts multiple times, or until the prevailing torque drops below some nominal value.

Some Bellevilles are designed so as to not exceed their yield strength when squashed completely flat, so would be hard to damage in that regard by tightening very hard.
 
I am watching this post for sometime and without dis-respect I am disappointed with the shallow discussion regarding Belleville spring selection and design. No one even mentioned that the theory and closed form design and analysis formulations or Belleville springs (cone disc springs) are well known for decades. Every engineering graduate student should be able to use those formulas to design a new spring and to check how an existing of off the shelf spring will fit the design goals.

When a Belleville spring is compressed to flat or even beyond flat, three types of stresses are usually needed to be taken into account. One is a compressive strength at the top inside diameter of the spring and the other two are tensile strength (one at the bottom large outside diameter and one at the top inside diameter of the disc). Therefore, for cyclic operation only the tensile stresses should be taken into account. However, most if not all Belleville spring manufacturing processes include a preset (scraging or set remove as it is sometimes called) process as that last process that induces favorable residual compressive stresses at the points where tensile stress governs the design. Therefore, much higher loads are able from such a spring compared to a spring that didn't include a preset process in it's manufacturing process.
 
israelkk,

I set up a spreadsheet using the Belleville spring equations from Roark's, and some similar equations from the SAE spring handbook. I wanted to design my own Belleville springs. As a sanity check, I pulled out my Schnorr catalogue, and I punched in their values. My spreadsheet and Schnorr were in fairly close agreement. I was happy.

Your preset would increase the maximum stress a bit, but the Schnorr washers can be compressed flat, according to my calculations. Couldn't you just punch them out of (fairly) soft metal and then heat treat them?

I wound up designing some delrin lens preloaders, and I left strict instructions to not compress them flat.

Critter.gif
JHG
 
Nice tutorial for our shallow minds israelKK, He now knows the theory behind how they are made, but you didn't answer the OP's question - how many times can he reuse his belleville washer?

rmw
 
rmw

Knowing the formulations, the loads and deflections on a spring, a competent designer can easily calculate/estimate the stresses and the fatigue life. To answer a question, preliminary specific data is needed including the spring dimensions, loads and deflections. The fact that none of this is given by trudels and your post proves my point.
 