Greetings!
I'm currently working on a job where we will be driving 9 5/8" OD x 0.472" pipe piles (open-ended) to refusal on bedrock at a depth varying from 3m to 23m. We have been given a safe design working load of 900kN/pile from our geotechnical consultant. As the piles are going to be driven open-ended, i was not going to concrete fill after installation. The piles will not be augered.
In a book by Joseph E. Bowles (Foundation Analysis and Design - 3rd Ed.), the author mentions that if the top of the pile is adequately embedded into the pile cap (say 150mm), a transfer plate is not necessary.
When i calculate the stress of the concrete on the area of the pile, i get a bearing stress of approximately 100MPa at the peak design load of the pile (!!!). Is there something i'm missing? Without concrete filling the pile, can you eliminate the transfer plate?
Thanks in advance for your time.
Regards,
Steve
==================================
Steve Cairns, M.A.Sc, P.Eng.
Halsall Associates
Sudbury, Ontario, CANADA
I'm currently working on a job where we will be driving 9 5/8" OD x 0.472" pipe piles (open-ended) to refusal on bedrock at a depth varying from 3m to 23m. We have been given a safe design working load of 900kN/pile from our geotechnical consultant. As the piles are going to be driven open-ended, i was not going to concrete fill after installation. The piles will not be augered.
In a book by Joseph E. Bowles (Foundation Analysis and Design - 3rd Ed.), the author mentions that if the top of the pile is adequately embedded into the pile cap (say 150mm), a transfer plate is not necessary.
When i calculate the stress of the concrete on the area of the pile, i get a bearing stress of approximately 100MPa at the peak design load of the pile (!!!). Is there something i'm missing? Without concrete filling the pile, can you eliminate the transfer plate?
Thanks in advance for your time.
Regards,
Steve
==================================