I need to understand the table in QW-423.1 page 131 of ASME Code Sec. IX, about the Base Material Qualification.
If I weld P1 to P1 pipe, am I qualified for to welder P1 to P11?
Or P1 to P11 and P34 and P41 through P47?

Thanks
Rdgs
Jean71
 
Replies continue below

Recommended for you

Jean71,
In the 2004 Edition of Section IX, QW-423.1 allows a welder to weld any combination of P1->P11, P34, and P41->P49 if P1->P1 is used for the initial qualification.
However, bear in mind that this holds true only if all other essential variables remain the same. This is not a free license for a WPQ within these P number ranges.