TankInspection1
Industrial
- Jul 7, 2006
- 1
I am attempting to evaluate Barcol hardness results from a FRP tank that has been in sodium chlorate solution service since 1995. The tank was constructed with inner corrosion barrier of DERAKANE 411 reinforced with (2) ply C-glass surface Mat.
From what I can ascertain the barcol hardness was approximately 35 when originally constructed and my average barcol hardness at this time is 39.78
What hardness value would indicate a potential problem for this type of equipment and service?
Thanks in advance for any assistance
From what I can ascertain the barcol hardness was approximately 35 when originally constructed and my average barcol hardness at this time is 39.78
What hardness value would indicate a potential problem for this type of equipment and service?
Thanks in advance for any assistance