Hi Members

For a pressure vessel built to ASME Sec VIII, is it allowed if shell (15mm thk ) circumferential joints with excessive root gaps upto 10 mm are welded by using temporary backing strips.Normally the excess root gaps are corrected by buttering the bevel ends.Joint detail is is single V with double side welding after back gouging.

Any inputs would be apprciated

Sree
 
Replies continue below

Recommended for you

Yes, backing for welding is allowed especially for removal to back gouge for full penetration welds.
 
you may want to consider using ceramic backing
 