Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations TugboatEng on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Backing bar design

Status
Not open for further replies.

ScooterMagee

Mechanical
Joined
Apr 25, 2001
Messages
2
Location
US
What parameters or standards determine the recommended design of the groove profile in a removable backing bar?
 
One important factor, is the access space for the welding gun, you must have a big enough gap which will permit you to weld at the root of your prepared joint and also have the right welding angle.
 
Welding backing bars are an off the shelf item at most welding supply shops.
AWS D1.1 requires that the composition and size be detailed on the WPS. Good Luck!