Dear all after i search and discussed another way of producing caustic soda and chlorine from salt, i am back to ion exchange membrane method. so i need your usual cooperation please.

i need to build the membrane cell so the first question will be can i use bare titanium and nickel metal for electrode without alloying them?
 