Jul 7, 2014 #1 cjgrass Industrial Joined Apr 8, 2013 Messages 34 Location US If the wps used for production welding requires PWHT is it required to perform PWHT on welder qualifications also? Is mechanical testing of performance tests per ASME IX required for section K?
If the wps used for production welding requires PWHT is it required to perform PWHT on welder qualifications also? Is mechanical testing of performance tests per ASME IX required for section K?
Jul 7, 2014 #2 DekDee Petroleum Joined Mar 12, 2012 Messages 1,324 Location PH cjgrass, Yes & Yes Regards, DD Upvote 0 Downvote