if your certified to ASNt level II for UT which meets AWS d.1 are there any additional requirements to examine welds fabricated under AWS d1.8
 
Replies continue below

Recommended for you

The Level II must be qualified per Annex E of AWS D1.8. The annex describes the practical examination and the test specimen that must be evaluated as well as the method of scoring the test results.

Best regards - Al
 