Hello,

In the syllabus for AWS CWEng exam, two surfacing process are mentioned as SW, THSP. Anyone have idea what it is?
Reference AWS B5. 16
 
You will find your answer in AWS A3.0 Standard welding Terms and Definitions. You'll need a copy if you plan on taking the CWEng examination.

Best regards - Al
 
SW - Arc Stud Welding
THSP - Thermal Spray

Best regards - Al
 
Thank you gtaw for the reply
 