They're basically the same as far as qualifying a PQR, WPS, and Welder Qualifications.
12472301 includes several Mil-Standards into it. Some of the old Mil-Standards didn't require PQRs (radiographic, tensile testing, etc.) It also includes armor.
Double-check the Codes for specific differences.
Keith