Base Material - ASTM A131- EH36 x 25.4mm (Thk) x Single V
Weld Process - SMAW / Weld Position - 3G-Uphill
All Mechanical Tests & Impact Testing( -20 deg celcius ) passed. But Hardness Value exceeds allowable range
Query:-
1) Is it mandatory( AWS D1.1 / ASME Sect IX )to conduct Hardness Test?
2) Does the PQR become void when hardness value exceeds allowable range?
Please share your expertise asap.