3
I have an existing weld procedure that is written IAW ASME and I would like to know what group of metal A519 falls under. Can someone help with this? Thanks.

Moose
 
Replies continue below

Recommended for you

AWS Classification
B2.1 2009
M-No 11B, Group 9
 
Thanks for the quick response.

If this material is used to qualify a procedure are all materials in groups 1-8 qualified as well?
 