Hi,

where can I find informations about AW 6056 (tensile strength, yield strength....)
 
Typical properties for alloy 6056-T6 are yield strength > 320 MPa, tensile strength = 380-450 MPa, elongation > 4%. The following are some references on applications using 6056-T6 and the mechanical properties:



 