I have a coded hair pin exchanger with general pitting. If certain pits are below tmin, what guidance should I follow for taking an average of the area? API 510 7.4.3? Can someone give me a quick understanding of general corrosion and pitting guidance that is a good practice to follow for understanding at what point further measures must be taken?
Also, if the hairpin exchanger is a 5" diameter and 30' long is this required to be a coded vessel (plant is in a non-coded state). All I have been able to locate is ASME Sect VIII regarding equipment greater than 6" must be coded and stamped.
Thank you