We are probably all aware of the universally adopted limit of 60 deg C as the threshold temperature for CSCC of 316/316L stainless steels; however, the limits for 6Mo austenitics are not so readily discernible. Does anyone using these materials have a specified threshold temperature for CSCC under atmospheric exposure (marine, industrial, whatever)?

Steve Jones