ASTM D1785 is used for water, I want to know if I can use this standard pipe for acid/alkali etc corrosive fluid. Thanks!
 
Replies continue below

Recommended for you

Yes. May consult with the PVC/CPVC vendor or Material Engineer for the pipe application for the service condition of your acid/alkali system, i.e. concentration, flow rate, P & T, etc.
 