astm C150

Status
Not open for further replies.

BigH

Geotechnical
Dec 1, 2002
6,012
Have there been any changes in the chemical or mechanical properties of portland cement from C150-04 until latest? Just wondering. Trying to compare a Russian Spec to ASTM
 
Replies continue below

Recommended for you

BigH....not any substantive changes. There is a push now to reduce some of the reference methods (autoclave expansion for instance), but changes between 2004 and now have been mostly editorial.

 