I believe the requirement of the above standard is that iron content shall not exceed the nickel content, what i ask is, if for some reason the iron content did exceed the nickel what would the implications be for material performance in terms of corrosion resistance, for example.
Does this question make sense? Sorry humble draughstman here but may have issue with some castings recently produced.
Does this question make sense? Sorry humble draughstman here but may have issue with some castings recently produced.