Hello everyone. I have this issue with a specification. I have this "ASTM B-62, UNS C-86300 smls pipe", and I was looking for a weight/schedule table and it seems pretty difficult to find. I also have some confusion about the spec itself, it is only for component castings of valves, flanges, and fittings, or can be used for pipes and tubes, or is just an error. Again, and as always, I appreciate your time
 
The scope states castings for valve components, flanges and fittings not for pipe. The smls pipe part of the quote above is in error.
 
thank you for the rapid response.
 
Normally, with bronze fittings and valves, I see ASTM B43 seamless brass pipe used.
 
ENG-TIPS ..... Geezers chasing typos for confused newbies

..... For the benefit of mankind !!!!

MJCronin
Sr. Process Engineer
 
Status
Not open for further replies.

Part and Inventory Search

Sponsor

Back
Top