I know ASTM withdrew A607 and A715 Gr. 50 material in the year 2000 and replaced it with A1011/A1011M, but is there still and is it possible for A715 available to purchased??

Mike
Chicago Metal Fabricators
 
Replies continue below

Recommended for you

You might find someone who still calls it A715, but why not just order A1011 HSLAS-F in whatever grade you need. This is the old A715.
 
Thanks for the input, but vendors still say it's A715 material. My next question is, "Is there any of it that still exist since it has so called been "withdrawn" in 2000?
 