Hi, great day,

Anyone, please help me out for an welding electrode for Casting of ASTM A352 Gr.LC2-1?

UTS:725-895 Mpa
YS:550 Mpa
Impact @ -73DegC 41J(Avg)

 
E10018M for the SMAW process. The LC2-1 composition for SA 352 contains 2.5-3.5% Ni, so you need to locate a filler metal or wire with a nominal composition of Ni, for starters, also with Cr and Mo for strength.
 
ER100S-1 or ER110S-1 would also work for you.
 
@metengr ,am afraid whether E10018M could bear impact @ -73DegC?
 
You try and qualify the WPS. If not, try E8018 C2, under matching in strength but is stated to meet 27 J at –75°C.
 