Jul 8, 2016 #1 Indra712 Materials Joined Jun 13, 2016 Messages 3 Location IN Hi all, Can we use ASTM A193 B7 material for U-bolts in piping supports (for CS, SS and Alloy 20 Pipes)- offshore platforms. What other materials can be utilized/ referred for this purpose? Thanks in advance. Indra712
Hi all, Can we use ASTM A193 B7 material for U-bolts in piping supports (for CS, SS and Alloy 20 Pipes)- offshore platforms. What other materials can be utilized/ referred for this purpose? Thanks in advance. Indra712
Jul 8, 2016 #2 metengr Materials Joined Oct 2, 2003 Messages 15,478 Location US Have you checked standards for offshore platforms? Upvote 0 Downvote