gjarvie-
Ok, ok, you said Table 2A, not 1A, so you mean Div. 2...
The allowable stresses for Div. 2 have not changed, thus the current allowable stress for SA516-70 material at 300°F is 22.5 ksi and at 400°F it is 21.7 ksi. Linearly interpolate intermediate values.
The new Div. 2 will have new, increased allowable stresses. My impression is that it will be issued as a 2005 or 2006 edition.
jt