Tek-Tips is the largest IT community on the Internet today!

Members share and learn making Tek-Tips Forums the best source of peer-reviewed technical information on the Internet!

  • Congratulations MintJulep on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASME Sect. IV Is figure HLW-415 (d) considered a "full pen" weld? Is it .85 JE?

Status
Not open for further replies.

jeevesme

Petroleum
Joined
Aug 7, 2011
Messages
64
Location
US
Our company requires that pressure vessel be built with a Joint Efficiency of a minimum .85, and if backing bars are used, they must be removed. The fab company sent me a few pages of section IV code with figure HLW-415 (d)and HLW-402 (a) highlighted. He said that this would result in a .85 joint efficiency. I am not familiar with IV, but just reading HLW-402, it doesn't seem to.

Any help is much appreciated.
 
E = 0,80 for Figure HLW-415 Heads Attached to Shells sketch (d) Butt Weld With One Plate Edge Offset

Regards
 
@r6155, that's what I was leaning toward. I contacted a colleague ealier and he thought it would be .85. I love codes.
 