ASME SEC VIII DIV 1 Vessel , Killed Steel

Status
Not open for further replies.

MOHAMMED89

Mechanical
Feb 25, 2015
85
Dear All,

Pressure Vessel as per ASME SEC VIII,Vessel Size is Dia 2m and length (Tan to Tan )4m Shell Material is A 516 gr 70, So wheather carbon steel plates shall be fully killed??? is there any code requirement for that?

Thanks in Advance :)
 
Replies continue below

Recommended for you

Thanks Weldstan :)

am asking about SA-516 gr 70, Hope 561 is typo error, However this fully killed is code requirement?? if you specify the clause then it will be more useful for me ??
 
Weldstan, Can you tell me which clause says this requirement?
 
4.1 "The steel shall be killed..." Then review Si content (minimum) in Table 1.
 