Hi,
Any one can guide me that, can we use ASTM A-53 B material instead of ASME SA-53 B material in hot water boiler ASME-IV? where all our registered dwgs. are according to SA-53 B!
If yes, do we have to do any documentation?
Pls. guide me ASAP.
Thanks
Mihir5577
 
Replies continue below

Recommended for you

Yes. Review ASME B&PV Code, Section II, Introduction, "Acceptable ASTM Editions". There is reference to using ASTM A 53 for SA 53.
 
Be careful.

The year of the ASTM Std. must be the same as listed in ASME SecII to be SA.

I would review the MTRs against the current SA spec. before I used the material. If the customer gave me a written OK..no problem.
 
ASTM uses A 53-B, ASME uses SA-53-B. There two standards are usually identical if they are issued the same year. They are the same material, however you should use SA materials for constructing ASME PVs or Boilers
 
In conjunction with all three of these posts,see the second to the last paragraph in the "Forward" of any Code section.
 
Xianglu,
The Code allows the use of a material spec; if the materials are the same anyone can use in Code Construction if the required procedure/cert by the mfr is followed.

other than that it is an agreement within the customer and the fabricator.
I have customers who will not allow the use of even SA53 materials.