Developing weld procedure SA240-2304 to SA240-2304 (P10H) (UNS-S32304)there is no reference to this material in ASME Sec IX (Table 422). ASME Sec II Part A Table 2 has reference to it. Can anyone let me know why it is not referenced in Section IX or was it referenced in later code edition.
 
Section IX 2013 has S32304 in Table 422 as a P-10H Gr. 1 in seamless and welded tube at 87ksi (>1") and at 100ksi (<=1") acc. to A/SA789, as well as seamless and welded pipe at 87ksi acc. to A/SA790.
 