My question is if a welder is qualified with a F3/F4 on 2" xxs and a F6/F5 (GTAW/SMAW) on 2" xxs would they also be qualified on F6/F4 (GTAW/SMAW).



I spoke with the local boiler and pressure vessel office and the "new" person responsible for welding doesn't seem to know for sure.
 
Yes, by virtue of the having the F3/F4(backing) and the F6/F5 (backing) welder performance qualifications.
 
He is qualified provided the employer has WPSs that support doing so.

Best regards - Al
 