My question is if a welder is qualified with a F3/F4 on 2" xxs and a F6/F5 (GTAW/SMAW) on 2" xxs would they also be qualified on F6/F4 (GTAW/SMAW).



I spoke with the local boiler and pressure vessel office and the "new" person responsible for welding doesn't seem to know for sure.
 
Replies continue below

Recommended for you

Yes, by virtue of the having the F3/F4(backing) and the F6/F5 (backing) welder performance qualifications.
 
He is qualified provided the employer has WPSs that support doing so.

Best regards - Al
 