Hello,

i would like to know that does asme b31.3 wall thickness equation can be valid to calculate tubing wall thickness (as heat exchanger tubing)

thank you in advance
 
Replies continue below

Recommended for you

Tubing; yes. Bit I guess it will depend on the application. HEX tubing would fall under VIII-1, process or instrument tubing would fall under B31.3.
 
If it's very thin wall tubing the D/t limit of 100 in B31.3 might be a problem .... applies to sif's and branch conn calcs etc.
 