Hello,

In ASME B31.3-2014 Table A-1, page 180, the "Notes" for the materials UNS no. S31254 (20Cr-18Ni-6Mo austenitic stainless steel) contains reference (8).

This note (8) to Table A-1 seems to pertain to carbon steels, low strength bolting and carbon steel bolting rather than austenitic steels.

Could this be a mistake?

I shall file a request to the ASME.