jte sent data from 1977 edition of B16.5 for A181-1 flanges. Need allowable pressure at 150F and 200F. thanks for the help.

JPG
 
ANSI 16.5 - 1977, Material Group 1.4 (A181-I)

Class 150: 235 psig @ 100 deg. F, 215 psig @ 200 deg. F.
Class 300: 620 psig @ 100 deg. F, 560 psig @ 200 deg. F.

For 150 deg. F. use linear interpolation.