Continue to Site

Eng-Tips is the largest engineering community on the Internet

Intelligent Work Forums for Engineering Professionals

  • Congratulations waross on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

ASME / ASTM SA/A 333 Gr. 6 Heat treatment

Status
Not open for further replies.

zebmahar

Materials
Dec 12, 2010
46
Hello Guys

According to ASME SA 333, Gr. 6 Product should be Quench and Tempered but we don't have the facility. Any how we do achieve the properties required by the said standard through simple heat treatment furnace. In your opinion, does our product qualify according to the standard?

Regards
 
Replies continue below

Recommended for you

zebmahar,
I always suspected the ASME SA 333 is a fake, but you just brought the proof;- you don't need to follow the standard requirements to manufacture the materials with the same properties. You also get a significant saving on the Q&T for your product. I congratulate you for your endeavour, but if I were you, I wouldn't rush to claim patent on your invention, I could hear a few giggles in the background.
Good luck,
gr2vessels
 
Quenching & tempering is not required for SA-333 Gr 6. Per 4.2.1.5, it "may be heat treated...followed by quenching in liquid and reheating to a suitable tempering temperature..."

You need to read all of 4.2.1.

 