Just as we have Table UCS 56.1 in ASME sec VIII Div 1, do we have a table or alternative provisions in 31.3 and 31.8 that permits lower soaking temperature compensated by higher soaking time.

 
Replies continue below

Recommended for you

Yes, see B31.3 Section (331) specifically,331.2.1 Alternative Heat Treatment, 2nd paragraph. For a lower PWHT temperature (an alternative method) you would need to qualify this method via hardness testing of a coupon or other, per the owner's satisfaction.
 