ASME Allowable Stress Values for Low Temperatures 4

Status
Not open for further replies.

Mark1arm

Mechanical
Joined
Sep 30, 2014
Messages
11
Location
GB
Does anyone know how to determine allowable stress values for low temperatures. I need to know what ASME states for design temperature if I am designing a vessel for operation at -196°C. For example: I am using SA240 304. the allowable stress (ATM) = 206.9 MPa, Allowable stress (DT ((@-196°C)) = ???
 
It is the same design stress.

At that temperature however, additional impact testing requirements will need to be addressed due to low temperature embrittlement.

Cheers,
 
The allowable stress for SA-240 304 at atmospheric temperature is 138 MPa not 206.9 MPa. There are increased low temperature allowables in table ULT-23.
 
Sorry should have mentioned I am referring to 1998 Ed. for CFR stress requirements.

Thanks for everyone's input on this!!
 
@Mark1arm,
I believe your question is addressed in General Note (e) for table 1A in II-D.

"(e) Stress values for -20°F to 100°F are applicable for colder temperatures when the toughness requirements of Section III,VIII, or XII are met."
 