I came across a comment which states that" All clad shell and head plates to be subjected to 100% UT after cladding per ASME A578 Acceptance level S6 class C, S1 &SA264 Class 1"
Vendor replay that SA264 is not appropriate as this applies to only bonded clad which is not being used as weld overlay s being used.Can someone please explain ? I try reading ASME578 but did not get any clue out of it. Just for eductation purpose . Thanks.
Vendor replay that SA264 is not appropriate as this applies to only bonded clad which is not being used as weld overlay s being used.Can someone please explain ? I try reading ASME578 but did not get any clue out of it. Just for eductation purpose . Thanks.