Eng-Tips is the largest forum for Engineering Professionals on the Internet.

Members share and learn making Eng-Tips Forums the best source of engineering information on the Internet!

  • Congratulations JStephen on being selected by the Eng-Tips community for having the most helpful posts in the forums last week. Way to Go!

Ash removal from shale oil ( heavy fuel oil + gasoline mixture)

Status
Not open for further replies.

balaji28

Civil/Environmental
Joined
May 1, 2003
Messages
18
Location
SE
Hi

I am looking for a suitable filter to treat 250 cu.m/hr of process media comprising of 85% heavy fuel oil and 15% gasoline.
The intent is to reduce ash content from inlet of 1000 ppm to outlet of 50 ppm.

I need to make a CAPEX and OPEX comparison for various filtration technologies

Appreciate recommendations

Regards

Bala
 
If I understand correctly, shale oil is generally made by pyrolysis of kerogen from the shale. It therefore should contain virtually no ash, i.e. no non-volatile inorganic matter originally present as dissolved in the "oil". If it does contain "ash", that would likely be dust from the shale rather than "ash" per se. Filtering 1000 ppm out of it is going to be quite costly because the particles could be very fine indeed.
 
in my knowledge:
- HFO + gasoline: no clear relation with shale oil;
- ash is generated thru the combustion of fuel oil by the salts (mainly chlorides of Na, Mg, Ca....) and metals (organometallic compounds with Fe, V, Ni....) originally included in the oil. you can't filter them. salts, but not metals, can be reduced by a desalting process (also removes sediments, if any).

questions:
- have you an analysis of the ashes (and salts, and BS&W, and metals)?
- which is the scope for reducing ashes?
 
Thanks for your reply

@ moltenmetal :It comes out as suspended solids and as you say could be dust. Was wondering a solution between filter cartridges or a high speed centrifuge(disc stack type), which should be better option.

@poli60 - I do not have the analysis. The reduction is to achieve 50 ppm from 1000 ppm
 
Try using a 2 step operation: Step 1 - hydrocyclones to knock out the bigger particles and most of the SS. Step 2 - a finer filter, Pall / Peco or similar filter cartridge.
A 2 step operation will extend the life of the stage 2 filters.
The reject stream from the hydrocyclones containing the suspended solids would need to disposed off somehow.
 
Thanks George
Would a high speed centrifuge ( disc stack centrifuge ) work after the hydrocyclone instead of filter cartridge ?
 
Dont think you need to go as far as a centrifuge. Expensive and high maintenance. To extend the life of the filters, would suggest setting up 2 stages of hydrocyclones. Talk to hydrocyclone vendors who can help you with this. Agreed, if the particles are too small, the hydrocyclones may not work as intended.
 