Are the pipes or materials of standard NACE MR0175 /MR0103 API5L Gr.B ...rust??
20190206_091023_ftsuup.jpg
20190206_090452_ao2107.jpg
20190206_090317_zbp7su.jpg
rust?
 
Yes, without costing protection, steel pipe will be rusted in the outdoor yard.
 
And depending on how long it has been in the sun the coating may be no good.
There are companies that do nothing other than clean improperly stored pipe.

= = = = = = = = = = = = = = = = = = = =
P.E. Metallurgy, Plymouth Tube
 
NACE carbon steel rusts but does not crack =)
 
Chunpes said:
NACE carbon steel rusts but does not crack =)
Give me some DMA and I'll make NACE carbon steel crack.

"Everyone is entitled to their own opinions, but they are not entitled to their own facts."
 