bhart192
Civil/Environmental
- Feb 6, 2006
- 81
we're planning to build a diffuser type box using AR 400 plate (1/4"), from my research we plan on using ER80s filler with perheat to 200 F and slow cool down. This box does not provide any structural support only used as a means to disperse material ,basically a duct system , AWS D1.1 requires 2 Tensile test , AR 400 has a yield of 140 ksi ,AWS requires a acceptable tensile test to meet the minimum yield of the base materials . if using ER 80s wire I can't see a tensile test reaching 140 ksi with the filler metal yield in the 80's. we want to use a low hydrogen filler . help