Hi,I'm looking for suggestions for a suitable Vacuum Breaker(s) for a 30,000 gal. stationary 29% Aqua Ammonia tank. We have had failures with Kunkle, Girard or DFT valves even though they are all 316 SS and suitable for ammonia service. I have looked at Johnson also, but this is located in an enviroment with up to 10 ppm SO2 concentration and the 440 SS ball is not suitable for SO2 service. 2-3" Hg rating would be a bonus.Any suggestions would be appreciated.Thanks
 
Replies continue below

Recommended for you

It seems the previous breakers were made of metals.
Assuming the failures were due to corrosion

Suggestion 1: FRP or PVC Conservation vent (Groth)

Suggestion 2: FRP or plastic Water vent pot.
 