Jun 18, 2010 #1 vanci Materials Joined Feb 18, 2002 Messages 62 Location US Can someone please recommend a filler metal for welding X70 grade steel? I am not going to use preheat or post heat treatment. I will also need solid wire in spool form for the GTAW process. Thanks in advance!
Can someone please recommend a filler metal for welding X70 grade steel? I am not going to use preheat or post heat treatment. I will also need solid wire in spool form for the GTAW process. Thanks in advance!
Jun 18, 2010 #2 stanweld Materials Joined May 9, 2003 Messages 2,906 Location US ER 80S-D2. Upvote 0 Downvote