Hello,
We are haing problems with single stage pumps that work with sour water (from crude oil desalators). Temperature: 120ºC
These pumps have single seal with flush plan 41, with cyclone separator and heat exchanger and the seals doesn't work properly as they leaking after few months. The flushing circulating doesn't seem to be good, as the temperatures doesn't follow a rational sequence.
I would be very grateful, if you had experience with this refinery service, if you could tell wich flush plan you use and your feelings about it.
I feel that plan 41 is not good and I would avouid the cyclone separator, as I do not have very good experience with this filtration element.
Any help will be greatly appreciated,
Marc
We are haing problems with single stage pumps that work with sour water (from crude oil desalators). Temperature: 120ºC
These pumps have single seal with flush plan 41, with cyclone separator and heat exchanger and the seals doesn't work properly as they leaking after few months. The flushing circulating doesn't seem to be good, as the temperatures doesn't follow a rational sequence.
I would be very grateful, if you had experience with this refinery service, if you could tell wich flush plan you use and your feelings about it.
I feel that plan 41 is not good and I would avouid the cyclone separator, as I do not have very good experience with this filtration element.
Any help will be greatly appreciated,
Marc