Hello,
Does anyone know the reasoning behind API653 11th ed 4.4.5.7 referring to the projection of the external chime outside of the shell-to-bottom weld being at least 3/8" ? It also says it must be at least 0.1" thick.
I'm asking since we have external corrosion on one tank leaving a chime of only 1/4" and now it looks like we must replace the bottom plates in this area. (Tank floor is butt welded without annular plates). I would like to know what purpose the 3/8" projection serves.
Thanks